Stress corrosion cracking

This particular type of corrosion occurs when a metal is under internal or external stress and at the same time under the action of a corrosive agent.

A distinction is made between intergranular corrosion (along the so-called "grain boundaries" of the structure) and transgranular stress corrosion cracking (corrosion that passes through the crystalline).

In the presence of a medium, e.g. water, the coating fails prematurely when external stresses occur.

This might also interest you ...

Other popular topics that are often clicked on include information on plastic finishing, metal finishing, chrome plating, galvanising, laser engraving or even tin plating:

Any questions? We’ll gladly assist you ...

Any questions?
We’ll gladly assist you ...

WIOTEC® Ense GmbH & Co. KG
Auf den Geeren 9-11
59469 Ense-Höingen, Germany

WIOTEC® Arnsberg GmbH & Co. KG
Wagenbergstraße 55
59759 Arnsberg, Germany

Phone
+49 2938 97833-0
Fax
+49 2938 97833-20
E-Mail
mailwiotec

From metal to precious metal
The company WIOTEC® is your specialist for surface finishing and metalworking. In our electroplating shop, which is managed according to the latest environmental standards, we are capable of finishing both small parts and long parts of up to six meters. This makes us one of the leading and most efficient decorative surface coaters in Europe.

Our most important resource is our employees - with their commitment, competence and experience. Together with them, we work out and develop individual and tailor-made solutions for our customers. From detailed consultation and planning to purchasing, mechanical and chemical pre-treatment, professional electroplating and supplementary services - WIOTEC®'s range of services leaves nothing to be desired.

© 2026 - WIOTEC® - ALL RIGHTS RESERVED.

© 2026 - WIOTEC® - ALL RIGHTS RESERVED.


Call us:

Stacks Image 343

Claudia Schäfer
+49 2938 97833-11

Or write to us:


Brochures, data sheets, etc.